電話:0755-23003036
電話:18123966210
郵箱:shirleywangfang@gmail.com
網(wǎng)址:http://www.zetuobio.com
QQ:343794406
QQ:286262992
General Information
Full name | Poly[(5,6-difluoro-2,1,3-benzothiadiazol-4,7-diyl)-alt-(3,3’’’-di(2-octyldodecyl)-2,2’;5’,2’’;5’’,2’’’-quaterthiophen-5,5’’’-diyl)] |
Synonyms | PffBT4T-2OD |
Chemical formula | (C62H88F2N2S5)n |
CAS number | 1644164-62-4 |
HOMO / LUMO | HOMO = -5.34 eV, LUMO = -3.69 eV [1] |
Solubility/processing solvents | Dichlorobenzene or Chlorobenzene+dichlorobenzene (1:1 v/v) at elevated temperature ca. 110 °C |
Classification / Family | Benzothiadiazole, Fluorinated benzothiadiazole, Heterocyclic five-membered ring, Organic semiconducting materials, Low band gap polymers, Organic Photovoltaics, Polymer Solar Cells |
Batch details
Batch number | MW | MN | PDI |
|
M301 | 117,490 | 54,900 | 2.14 | |
M302 | 172,033 | 83,008 | 2.07 | |
M303 | 112,707 | 55,674 | 2.02 |
|
Applications
PffBT4T-2OD (PCE11) is a low band-gap (1.65 eV) semiconducting polymer for organic photovoltaics (OPVs), which has reached power conversion efficiencies (PCEs) approaching 11% [1]. These efficiencies are a result of the high crystallinity of the polymer, providing excellent hole transport mobilities on the order of 10-2 cm2V-1s-1, and the ability to use a thick active layer, resulting in improved light absorption.
The size and position of the alkyl chains of PffBT4T-2OD are critical to its temperature dependant aggregation properties, enabling control over the aggregation and crystallisation of the polymer to produce an efficient donor:acceptor film morphology.
Polymer PCE11 was targeted by reacting 4,7-bis(5-bromo-4-(2-octyldodecyl)thiophen-2-yl)-5,6-difluorobenzo[c][1,2,5]-thiadiazole with 2,5-bis(trimethylstannyl)thieno[3,2-b]thiophene engaging Stille Coupling reaction.
PCE11 (PffBT4T-2OD) synthesis with 4,7-bis(5-bromo-4-(2-octyldodecyl)thiophen-2-yl)-5,6-difluorobenzo[c][1,2,5]-thiadiazole with 2,5-bis(trimethylstannyl)thieno[3,2-b]thiophene as starting materials engaging Stille Coupling reaction.
Usage Details
The structure of the high-performance (10 - 11%) devices was:
ITO / ZnO / PffBT4T-2OD:PC70BM (200 – 300 nm) / MoO3 or V2O5 (20 nm) / Al (100 nm)
PffBT4T-2OD:PC70BM solution details:
- Blend ratio: 1:1.2,
- Polymer concentration: 9 mg/ml,
- Solvent: 1:1 blend of chlorobenzene and dichlorobenzene,
- Additive: 3% diiodooctane,
- Heating: 85°C for dissolution,
It is important to note that this solution (and the substrate being deposited onto) must be heated for spin casting, with the ideal temperature being 60 – 80°C. It is reported that a solution and substrate pre-heating temperature of 110°C should be used to allow for cooling that will occur before deposition.
Literature and Reviews
- Aggregation and morphology control enables multiple cases of high-efficiency polymer solar cells, Y. Liu, et al., Nat. Comm., 5, 5293 (2014)
- High-efficiency non-fullerene organic solar cells enabled by a difluorobenzothiadiazole-based donor polymer combined with a properly matched small molecule acceptor, J. Zhao et al., Energy Environ. Sci., 8, 520-525 (2015)